Mechanical Characteristics |
Tensile stress at yield |
MPa |
ISO 527-1,2 |
85 |
Tensile strain at break |
% |
20 |
Tensile modulus |
GPa |
3.2 |
Flexural strength |
MPa |
ISO 178 |
110 |
Flexural modulus |
GPa |
2.7 |
Charpy notched impact strength |
kJ/m2 |
ISO 179-1/1eA |
5 |
Rockwell hardness |
R.Scale |
- |
ISO 2039-2 |
120 |
M.Scale |
80 |
Thermal Characteristics |
Melting temperature |
°C |
ISO 11357 |
215~225 |
Coeff. of linear thermal expansion |
x10-5/°C |
ISO 11359-2 |
8 |
Temperature of deflection under load |
0.45 MPa |
°C |
ISO 75-1,2 |
175 |
1.8 MPa |
°C |
66 |
Electical Characterisitics |
Volume resistivity |
Ωcm |
JIS K6911 |
1015 |
Electric strength |
kV/mm |
IEC 60243-1 |
20 |
Relative permittivity |
- |
IEC 60250 |
3.5 |
Arc resitance |
s |
D-495(ASTM) |
119 |
Others |
Density |
g/cm3 |
ISO 1183-3 |
1.14 |
Water absorption |
23 °C, 50 %RH |
% |
UBE method |
2.7 |
Molding shrinkage |
MD |
% |
UBE method(30x100x3t) |
1.2 |
TD |
1.3 |
Nomenclature according to ISO 16396-1 |
|
|
PA6, M1R, S12-030N |